Polystyrene VerticalPFM INSPParis Chloroform Electrode Blood Pipette SelfAssembly Mapping Mosfet CalciumHydroxide Lateral SiliconOxide Workfunction CP-AFM Aluminium_Oxide ElectrostaticForceMicroscopy Cobalt Gold neodymium_magnets PVAC AnodizedAluminumOxide #EC Alloy non_contact Spincast cannabidiol exfoliate InorganicCompound Permalloy suspended_graphene block_copolymer PECurve Silicon Treatment
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512