LiNbO3 Biofilm Dimethicone Nickel Graphene CastIron PtfeMembrane PinpointPFM UTEM epitaxy temp_control C36H74 CalciumHydroxyapatite ChemicalCompound Ananth HighResolution EFM MechanicalProperties TyphimuriumBiofilm Al2O3 HBN ULCA polyvinyl acetate chemical_compound Adhesion Solution OpticalWaveguide BloodCell FAPbI3 Christmas I-VSpectroscopy FrictionalForce AdhesionEnergy TungstenDeposition NCM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256