Aluminium_Oxide vertical_PFM BlockCopolymer Polyvinylidene_fluoride Corrosion Composition AM_KPFM HBN Memory Layer LaAlO3 YszSubstrate MESA structure Ceramics temperature_control food SKKU Celebration Litho Hexatriacontane Chungnam_National_University TPU Spain Croatia Ananth 3-hexylthiophene Typhimurium Chloroform OpticalWaveguides Biology Permalloy Styrene Iron InsulatorFilm FrequencyModulation
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256