FAPbI3 Glass VortexCore PatternedSapphireSubstrat Topography HexagonalBN Metal BaTiO3 VerticalPFM GaN molecular_self_assembly PDMS Nanopattern StyreneBeads LogAmplifier Mechanical&nanotechnology MagneticForce Modulus Alkane Piezoresponse ForceVolumeMapping PECurve OpticalElement Optical alkanes pinpoint mode MoS2 BloodCell Spain AM_SKPM amplitude_modulation ElectroDeposition KPFM Conductivity Imprint
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Imprint sample
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 20μm×20μm
- Scan Rate:0.25Hz
- Pixel: 256×256