Layer AlkaneFilm FM_KPFM Growth FloppyDisk NUSNNI mechanical property MESA structure GlassTemp IISCBangalore SurfaceOxidation Pzt ScratchMode cannabinoid Hole self_assembly Korea ContactModeDot Implant Monisha LightEmission FuelCell TyphimuriumBiofilm graphene_hybrid BTO Nanostructure Hafnium_dioxide BloodCell silicon_carbide Ceramics HafniumDioxide Scanning_Thermal_Microscopy Polyethylene FrequencyModulation cooling
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BFO (BiFeO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 5μm×5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512