Fujian H-BN MagneticForce MagneticPhase IIT-chennai Magnetic Force Microscopy SKKU StainlessSteel FAPbI3 Fe_film Silver 2-vinylpyridine Nanotechnology HighResolution Heat EFMAmplitude small_scan light_emitting gallium_nitride SingleCrystal fluorocarbon PetruPoni_Institute Ferrite GlassTemperature Layer Singapore HexagonalBoronNitride Sapphire plastics IndiumTinOxide HighAspect ForceVolumeImage PolyimideFilm Graphene DeflectionOptics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256